Physical Properties Metric English Comments
Specific Gravity 0.668 - 0.672 g/cc
0.668 - 0.672 g/cc
ASTM D287
LG Chemical Raw C5
Structure & Characteristics: Synthesized by vacuum-distillation of pyrolysis gasoline produced from naphtha pyrolysis process. The content of isoprene as C5 without undergoing hydration process is h..
Specific Gravity 0.668 g/cc
0.668 g/cc
300°C
ChevronTexaco 46 Heat Transfer Oil
FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont..
Specific Gravity 0.668 g/cc
0.668 g/cc
300°C (572°F)
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..