Polymer Property : Specific Gravity = 0.630 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.630 g/cc
0.630 g/cc
LG Chemical C5 Product
Structure & Characteristics: Obtained as a by-product from pyrolysis oil hydration plant which was produced from naphtha pyrolysis process, and C5 content is higher than 95%. Although it is in liqui..
Specific Gravity 0.630 g/cc
0.630 g/cc
ASTM D3574
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness)
AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Specific Gravity 0.630 g/cc
0.630 g/cc
ASTM D792-66
BCC Products LIK-WOOD BC 8007 Urethane Casting
Lik-Wood is a low viscosity, quick setting, easy to use casting material. A model or tool cast from Lik-Wood will weigh 60% less than other filled urethane systems. Within 30 minutes after mixing an..
Specific Gravity 0.630 - 0.720 g/cc
0.630 - 0.720 g/cc
Cos40 Cork/Neoprene Rubber Sheet
Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot..