Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.519 g/cc | 0.519 g/cc | ASTM D792 |
PolyOne Maxxam™ SY 89-22-7 Polypropylene, Unspecified (PP, Unspecified) Maxxam ™ SY 89-22-7 is a polypropylene copolymer compound with a pre-dispersed blowing agent for up to 60% expansion. The compound offers consistent cell structure, dielectric properties, and stren.. |