Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.420 g/cc | 0.420 g/cc | ASTM D3574 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Specific Gravity | 0.420 g/cc | 0.420 g/cc | ASTM D3574 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |