Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.220 g/cc | 0.220 g/cc | foam |
Kuraray HYBRAR® F2 Foam Compound Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Specific Gravity | 0.220 g/cc | 0.220 g/cc | ASTM D3574 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |