Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.160 g/cc | 0.160 g/cc | |
BCC Products MB 1100 Polyurethane Foam Modeling Board MB 1100 is an Olive colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1100 is low density foam of approximately 10lbs/ft3 board. Easily cut using CNC machining equipment or .. |