Polymer Property : Brookfield Viscosity = 970 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 970 - 2500 cP

@Temperature 25.0 °C
970 - 2500 cP

@Temperature 77.0 °F
7000 Adhesive; LVT, Spindle #3 @ 30rpm
Lord Adhesives Flocklok® 7000/7204 Flock Adhesive
LORD Flocklok® 7000/7204 adhesive is a two-part, single-coat adhesive used for adhering polyester or nylon flock fibers to a variety of thermoplastics, including PVC, Alcryn®, Sunprene®, ny..