Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 80 cP @Temperature 25.0 °C |
80 cP @Temperature 77.0 °F |
K3425A; RVT, spindle #2 @ 10rpm |
Lord Adhesives Aeroglaze® K3425 Sandable Primer/Surfacer For application on epoxy graphite or other plastic substrates or over a suitable primer on metal.Limitations - Aeroglaze® K3425 primer/surfacer contains no inhibiting pigments and is not suitable.. |