Polymer Property : Brookfield Viscosity = 75000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 75000 - 110000 cP

@Temperature 25.0 °C
75000 - 110000 cP

@Temperature 77.0 °F
3236 (Top); Spindle #7 @ 20rpm
Lord Adhesives Metech 3233 / 3236 Two Part Conductor System
Two part silver termination system for use on P.T.C. thermistor bodies. 3233 is the ohmic contact bottom coat and 3236 is the solderable silver top coat. These materials are screen printable and are..