Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 230000 - 690000 cP @Temperature 25.0 °C |
230000 - 690000 cP @Temperature 77.0 °F |
310B Hardener; HBF, Helipath @ 5rpm |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |