Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 450000 - 2.00e+6 cP @Temperature 25.0 °C |
450000 - 2.00e+6 cP @Temperature 77.0 °F |
322 Hardener; HBF, Helipath @ 5rpm, T-Bar Spindle E |
Lord Adhesives 320 / 322 Epoxy Adhesive LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides .. |