Polymer Property : Brookfield Viscosity = 2850 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 2850 cP

@Temperature 190 °C
2850 cP

@Temperature 374 °F
ASTM D3226
Westlake Epolene® C-16 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified
Product Description: Epolene C-16 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and..
Brookfield Viscosity 2850 cP

@Temperature 190 °C
2850 cP

@Temperature 374 °F
Westlake Epolene® C-16P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-16P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and..