Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 16650 cP @Temperature 125 °C |
16650 cP @Temperature 257 °F |
ASTM D3226 |
Westlake Epolene® C-16 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified Product Description: Epolene C-16 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and.. |
|||
Brookfield Viscosity | 16650 cP @Temperature 125 °C |
16650 cP @Temperature 257 °F |
|
Westlake Epolene® C-16P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-16P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and.. |