Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 14250 cP @Temperature -26.0 °C |
14250 cP @Temperature -14.8 °F |
|
ChevronTexaco RPM® SAE 50 Synthetic Transmission Fluid FeaturesChevron RPM Synthetic Transmission Fluid is a heavy duty truck manual transmission fluid.It is manufactured from synthesized hydrocarbon base fluids which have excellent thermal and oxidatio.. |