Polymer Property : Brookfield Viscosity = 1250 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 1250 cP

@Temperature 0.000 °C
1250 cP

@Temperature 32.0 °F
ChevronTexaco RPM® SAE 50 Synthetic Transmission Fluid
FeaturesChevron RPM Synthetic Transmission Fluid is a heavy duty truck manual transmission fluid.It is manufactured from synthesized hydrocarbon base fluids which have excellent thermal and oxidatio..
Brookfield Viscosity 1250 cP

@Temperature 0.000 °C
1250 cP

@Temperature 32.0 °F
ChevronTexaco Syn-Star® TL SAE 50
Texaco Syn-Star® TL delivers value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oil used in this product provides outstanding stability.Extended drain capabil..