Polymer Property : Brookfield Viscosity = 1.10e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 300000 - 1.10e+6 cP

@Temperature 25.0 °C
300000 - 1.10e+6 cP

@Temperature 77.0 °F
309-1D Resin; HBF with Helipath and T-C @ 5rpm
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive
Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh..