Polymer Property : Spiral Flow = 9.20 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 23.4 cm
9.20 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar
LyondellBasell Alathon® M4621 High Density Polyethylene
ApplicationsALATHON M 4621 is a copolymer that provides outstanding stress crack resistance and low temperature impact strength. Typical applications include small two-piece engine gas tanks, waste..