Physical Properties Metric English Comments
Spiral Flow 59.0 - 83.0 cm
23.2 - 32.7 in
177°C/1000 psi
Cookson Group Plaskon® 3400FP Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A fast curing, reduced-stress epoxy molding compound for the encapsulation of semiconductor devices including DIPs, PLCCs, SOICs ..