Polymer Property : Spiral Flow = 78.7 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 78.7 cm
31.0 in
PolyOne Geon™ 80520 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 78.7 cm
31.0 in
PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne