Spiral Flow 700 cm
276 in
AKRO
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry  (discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..