Polymer Property : Spiral Flow = 7.10 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 7.10 cm

@Load 750 kg,
Temperature 320 °C
2.80 in

@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
Kuraray Genestarâ„¢ GW2458HF Nylon, 45% Glass Filled
Low Warpage, High Flow V-0 Grade. It is suited for low warpage and high flow applications, making it well suited for card connectors.