Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 8.50 - 63.0 cm | 3.35 - 24.8 in | Average value: 21.7 cm Grade Count:14 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |