Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 62.0 cm | 24.4 in | |
Kraton® G1652 + PP blend (20/80) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Spiral Flow | 62.0 cm @Temperature 220 °C |
24.4 in @Temperature 428 °F |
ASTM D3123 |
Total PS CPDS 815 High Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 815 is a high heat resistant, high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stab.. |