Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 58.4 - 61.0 cm | 23.0 - 24.0 in | Average value: 59.1 cm Grade Count:4 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |