Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 60.0 cm | 23.6 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Spiral Flow | 60.0 - 85.0 cm | 23.6 - 33.5 in | Average value: 68.3 cm Grade Count:3 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |