Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 55.9 cm
22.0 in
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 55.9 cm
22.0 in
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..