Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 15.0 cm @Thickness 1.00 mm |
5.91 in @Thickness 0.0394 in |
380°C nozzle, 180°C tool |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |