Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 45.7 cm | 18.0 in | NOVA Snake Flow Test |
NOVA Chemicals Sclair® 2318 LLDPE Injection Molding Resin
(discontinued **) Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Applications: Thin walled container lids and closures.Data provided by the manufacturer. |