Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 40.0 cm | 15.7 in | AKRO |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Spiral Flow | 40.0 cm | 15.7 in | AKRO |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |