Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 4.10 cm | 1.61 in | |
Tipco Tipcolite® TPF 550 - Unreinforced Phenolic Resin having 41 mm Norton Flow with 9% Hexamine Unreinforced Phenolic Resin having 41mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd.,
Ind.. |