Polymer Property : Spiral Flow = 4.00 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 4.00 cm
1.57 in
Tipco Tipcolite® TPF 1110 - Unreinforced Thermoset Phenolic Resin, 40mm Norton Flow with 9% Hexamine
Unreinforced Phenolic Resin having 40mm Norton Flow, in Powder FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd., India.