Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 72.0 cm | 28.3 in | 165°C/1000 psi |
Cookson Group Plaskon® PPF-165A Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A conventional molding compound specifically formulated for semiconductor devices which are molded with preplated leadframes. Lo.. |
|||
Spiral Flow | 72.0 cm | 28.3 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Spiral Flow | 72.0 cm | 28.3 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |