Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 71.1 cm | 28.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 71.0 cm @Thickness 2.50 mm |
28.0 in @Thickness 0.0984 in |
at 255°C melt temp. |
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Spiral Flow | 71.0 cm @Thickness 2.50 mm |
28.0 in @Thickness 0.0984 in |
at 254°C melt temp. |
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |