Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 68.6 cm | 27.0 in | |
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 68.6 cm | 27.0 in | |
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |