Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 55.0 - 65.0 cm | 21.7 - 25.6 in | Average value: 60.7 cm Grade Count:6 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |