Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 22.7 cm @Thickness 1.00 mm |
8.94 in @Thickness 0.0394 in |
recommended processing conditions |
Victrex® PEEK 150PF Easy Flow Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, .. |