Spiral Flow 57.4 cm
22.6 in
Kraton® G1650 + PP blend (20/80)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..