Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 21.8 cm | 8.60 in | Equistar test |
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case.. |