Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 19.8 cm | 7.80 in | Equistar test |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |