Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 31.5 cm | 12.4 in | Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar |
LyondellBasell Alathon® M5040 High Density Polyethylene ApplicationsALATHON M 5040 is a copolymer with broad molecular weight distribution. This resin exhibits excellent color, low odor, and good processing stability. Typical applications for this res.. |
|||
Spiral Flow | 31.5 cm | 12.4 in | Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar |
LyondellBasell Alathon® M5562 High Density Polyethylene ApplicationsALATHON M 5562 is a copolymer with medium molecular weight distribution. This resin provides moderate stiffness, toughness and stress crack resistance. Typical applications include noz.. |