Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 26.7 cm | 10.5 in | Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar |
LyondellBasell Alathon® M6580 High Density Polyethylene ApplicationsALATHON M 6580 is a narrow molecular weight distribution homopolymer that enhances processability and stiffness, exhibits excellent color, low odor and good processing stability. Typica.. |