Polymer Property : Linear Mold Shrinkage, Flow = 0.037 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.037 cm/cm
0.037 in/in
ASTM D955
PolyOne Gravi-Tech™ GT5200-0002 Black Polypropylene Alloy (PP Alloy)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.037 cm/cm
0.037 in/in
ASTM D955
PolyOne Gravi-Tech™ GRV-TP-050-CU-NAT Styrene Butadiene Block Copolymer (SBC)
Information provided by PolyOne