Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0335 cm/cm @Thickness 3.17 mm |
0.0335 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GF/M40 HS L NAT 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Linear Mold Shrinkage, Flow | 0.0335 cm/cm @Thickness 3.17 mm |
0.0335 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GF/M40 L BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |