Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0223 cm/cm @Thickness 2.00 mm |
0.0223 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Leneâ„¢ LD1630J Low Density Polyethylene Injection Molding Key Characteristics:Good flowability for multicavitiesGood toughness and flexibilityExcellent gloss and transparencyOdorlessSafe for food contactRecommended Applications:HousewaresSmall to large clo.. |