Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0185 - 0.0215 cm/cm | 0.0185 - 0.0215 in/in | |
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |