Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0202 cm/cm @Thickness 2.00 mm |
0.0202 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |