Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0158 - 0.0198 cm/cm | 0.0158 - 0.0198 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1573-N Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |