Polymer Property : Linear Mold Shrinkage, Flow = 0.01651 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.01651 cm/cm
0.01651 in/in
ASTM D955
Styrolution Styrolux® 3G46 SBC
Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im..