Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0144 cm/cm

@Thickness 2.00 mm
0.0144 in/in

@Thickness 0.0787 in
TPE Method
SCG Chemicals EL-Proâ„¢ P842J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityExcellent stiffnessSuitable for complex parts and large partsRecommended Applications:Electrical appliance parts, mainly for refriger..