Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0128 cm/cm @Time 86400 sec |
0.0128 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific) This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region. |